FACTORY DIRECTOEM & CUSTOMEXPORT READYMIXED CONTAINER
300+Containers Shipped Since 2016
4 x 40'FCLMonthly Capacity
1 x 20'FCLMinimum Mixed Container
12 WeeksTypical Lead Time
Manufacturer & Exporter of Teak Root Furniture · Established 2016 · Jepara, Indonesia · Shipping Worldwide
Teak Root Furniture Manufacturer for European Importers

Teak Root Furniture Manufacturer for European Importers

Handcrafted teak root furniture from Jepara, Indonesia. Indoor and outdoor collections for wholesale and export buyers.

Sculptural Teak Root Dining Tables

Sculptural Teak Root Dining Tables

Solid teak root and glass-top dining tables, produced to order and prepared for container shipment.

Organic Coffee and Side Tables

Organic Coffee and Side Tables

Natural root-base coffee and side tables — statement pieces for retail and interior projects.

Wholesale and Custom Production

Wholesale and Custom Production

Custom and OEM production for importers, retailers and hospitality projects worldwide.

Request Our Catalogue and Price List

Request Our Catalogue and Price List

Send us your target items and quantities — our team will prepare a quotation for you.

Monday, November 23, 2026

Moisture Content and Cracking in Teak Root Furniture

Summary: Teak root cracks when it ships wetter than the room it lands in. We dry every top to a 10–12% band, check it with a pin meter at nine points, and write the destination band into the PO. From our list: Cabak dining table 120 cm, 1.08 CBM at USD 265 FOB; Mawar coffee table 100 cm, 0.45 CBM at USD 115; a 20ft takes 22 CBM inside 23.8; MOQ one 20ft mixed container; lead time 12 weeks from Jepara.

A buyer opens a container in Rotterdam in February and finds hairline splits at the ends of four dining tops. Nothing was dropped. The kiln report says 11%. The room those tables are going into sits at 28% relative humidity for three months. Both numbers are true, and the gap between them decides the claim.

Mawar teak root coffee table 100 cm with a flattened, oiled top

Why a root top cracks and a plank does not

Wood shrinks unevenly as it dries, roughly twice as much across the growth rings as along the rays. Published teak figures put total tangential shrinkage near 5.8% and radial near 2.5% from green to oven-dry. A plank has one direction to fight. A top cut across a stump has both, on the same face.

On a 120 cm round top, a four-point drop in moisture costs about 10 mm tangentially and 4 mm radially. The difference goes into a check at the end of a growth ring, which is exactly where you see it on arrival.

The root is not a straight column

Root fibre turns. It spirals around stones, splits around a bark pocket and reacts to the load the tree carried. That is why root dries slower and less predictably than a sawn board of the same thickness, and why a schedule built for straight stock will tear it.

None of this is a defect. Drying it like a plank is.

What the number means at the destination

Wood settles at an equilibrium moisture content set by the air around it, and that equilibrium differs in Osaka, Denver and Copenhagen in January.

Service environmentRH rangeEquilibrium MC
Heated interior, northern winter25–35%5.5–7%
Air-conditioned interior45–55%8–10%
Coastal temperate, covered terrace60–70%11–13%
Tropical humid, open air80–85%16–18%

Our 10–12% band suits air-conditioned interiors and covered terraces, where most of our volume goes. It is deliberately not the wettest possible reading, because a top packed at 16% and landed in a Dubai apartment will lose ten points and open up. For a heated northern interior, ask for 8–10% and expect a longer kiln cycle.

Too wet gives cracks on arrival, visible and expensive; too dry gives swelling in a humid market, slowly and usually blamed on the retailer. The PO should name the destination, not just a percentage.

How we dry a root top

Air first, kiln second

Root comes out of the ground at fibre saturation and above. Stacking it under cover with stickers and airflow for weeks removes free water cheaply and lets growth stress relax before any heat. Going straight to the kiln case-hardens a slab: dry outside, wet inside, and certain to crack later.

A schedule built for thickness

Drying rate is governed by how far moisture has to travel, so a 6 cm top and a 12 cm top never share a schedule. We start with a low dry-bulb and a wide wet-bulb depression, raise temperature only after the core reading falls, and finish with an equalising hold so shell and core meet within a point or two. The final conditioning stage relieves case-hardening; without it a top can measure correctly and still cup a month later.

Cabak teak root dining table 120 cm, single slab top on a root base

Measuring on the slab

A pin meter is practical and imperfect. On root the pins meet extractives and dense latewood, so readings can run two to four points low against an oven-dry test on a cut-off. Three habits keep it honest: nine points per top, a meter corrected for temperature and species, and one oven-dry check per lot at 105 °C.

Check or crack: where the accept line sits

Every root top shows something after a sea voyage. The question is which somethings are normal. This is our final-inspection table — agree it with your own QC before the first container.

FindingWhat it looks likeVerdict
Surface checkHairline, under 1.5 mm wide, a third of thicknessNormal; wax fill if visible
End checkRuns in from the end, stops inside the topAccept with note; stabilise
Through-crackFull thickness; light visible from belowReject and replace
Ring shakeSeparation along a ring, hidden until sandedReject; it will open
Loose bark pocketBark or grit sitting in a voidClean, fill with tinted epoxy
Raised grainFibre proud where the grain turnsSand to 220; not a defect

Measure a check across its width with a feeler gauge and record it in millimetres. Agree the accept line in writing before production; a buyer who discovers it after loading has no lever.

Stopping a live check

A check that is still opening must be arrested, not filled. On wide tops we cut a bowtie key across the split, glue it in with epoxy and flatten; where a key would look wrong, a steel bar goes into a channel underneath. Wax alone buys a season.

The container is a humidity chamber

Between Jepara and a European port a container crosses climate zones and cycles daily. Steel heats, air cools at night, moisture condenses on the roof and drips onto the load. That is container rain, and it is why a top packed at 11% can arrive with mould or fresh checks.

Three rules follow: line the container with kraft paper rather than sealing cartons in plastic; hang desiccant bags sized to the cubic metres loaded; leave tops in breathable wrap.

Console 150 cm teak root table, narrow top with end grain exposed at both ends

What our model list says about exposure

Risk is not evenly spread. Small tops expose more end grain per cubic metre and move sooner; large tops carry more internal stress but far more wood per unit of freight. Eight models from our list, with FOB per CBM derived by dividing price by volume:

ModelSizeCBM/pcFOB USDFOB per CBM
Karang Coffee Table100 × 50 cm0.20115575
Coffee Table120 × 60 cm0.29135466
Yava Coffee Table100 × 100 cm0.40115288
Lemma Coffee Table120 × 120 cm0.40110275
Mawar Coffee Table100 cm0.45115256
Cabak Dining Table120 cm1.08265245
Oval Root Dining Table200 cm1.50365243
Mawar Dining TableØ 150 cm1.69340201

Small coffee tables earn far more per cubic metre than large ones, but expose more end grain per dollar of freight, so crack risk per cubic metre is higher. Our mixed 20ft plans therefore load small pieces lower in the stack.

Clause for the purchase order

Take the wording. A clause that names a band, a method and a sample size is enforceable; "kiln dried" is not.

All visible surfaces to be 10–12% moisture content at time of packing, measured with a calibrated pin meter at nine points per top and recorded per piece; one oven-dry check per lot; spread across any single top not to exceed 1.5 points; no through-cracks or ring shake; surface checks under 1.5 mm accepted without concession; container to be lined and desiccant-hung.

Request FOB prices and a load planBuild a container load →

Frequently asked questions

Is 12% moisture content dry enough for teak root furniture?

For air-conditioned interiors and covered terraces, yes. For a heated northern winter at 30% humidity, ask for 8–10%.

Will a small check in the top get worse?

Not if it is a surface check under 1.5 mm on an equalised top. A check still opening in the first weeks points to a gradient across the thickness and should be keyed, not filled.

Does a heavier table mean wetter wood?

Not reliably; root density varies piece to piece. Nine pin-meter points plus one oven-dry check per lot separates a dense top from a wet one.

Can you dry to a specific band for a project?

Yes, inside 8–12%. Tighter costs kiln time and adds days to the 12-week lead time, so tell us at enquiry. A Cabak 120 cm stays 1.08 CBM and USD 265 FOB.

Written by

Mr. August Praymunor — Overseas Marketing Director

CV. Nusantara Sourcing Agent · manufacturer and exporter of teak root furniture in Jepara, Central Java, Indonesia. We have shipped over 300 containers since 2016, loading 4×40’FCL per month for importers, hotel groups and interior contractors in Europe and North America. Every price and volume in this article comes from our own model list and shipping records.

export@teakrootfurniture.com · WhatsApp +62 852 0600 7878 · LinkedIn · Jl. RA Rukmini KM.02 Pekalongan RT.02/V, Tahunan, Jepara 59428, Central Java, Indonesia

Share this page:

FAQ: Sourcing Agent & Factory Visits

Do you provide sourcing-agent services or factory visits?

We manufacture and export our own furniture from Jepara, Indonesia. We do not run a sourcing-agency service (no daily fee, no commission, no multi-supplier tours). Buyers/importers are welcome to visit our workshop; for products outside our lines we can consolidate and cooperate with other suppliers.

0 comments:

Post a Comment