Summary: On teak root furniture the finish is the only non-structural specification: a sanding schedule, a penetrating oil, or a pigment wash. Natural is bare sanded wood; honey is oil that keeps the warm tone; black-wash is pigment in a binder. None changes packed volume or FOB — a Mawar Ø 150 cm stays 1.69 CBM / USD 340 in all three, and a 20ft still loads 14 pieces at 23.8 CBM. MOQ one 20ft mixed container, lead time 12 weeks from Jepara.
Three buyers ask for the same dining table and each names a different finish. One wants it “natural”, one wants “the honey colour from your website”, one sends a photograph of a near-black root with pale grain showing through. In the workshop these are three processes with three drying times and three failure modes — and only one is a colour decision at all. Here is what goes on the wood, where each one fails, and how to write it on a purchase order.

Natural: bare wood, and nothing else
Natural means the piece leaves the sanding room with no oil, wax or pigment on it. It is not “unfinished” in the sense of rough — it is sanded through a fixed schedule and then left alone.
Teak root arrives at the bench as a chain-sawn block full of soil, bark pockets and decayed fibre. We flatten the top, then work 40, 80, 120 and 180 grit, finishing at 220 on visible faces. Skipping a grit stays visible for years: a 120-grit scratch under a 220 surface opens into a dark line as the wood takes up moisture.
Natural is also the most demanding finish on the material. There is no pigment to even out heartwood against sapwood, so grain, mineral streaks, small checks at the end of a slice and the odd blue-grey soil stain all stay visible. Voids must be specified too: left open, filled with clear epoxy, or filled with black epoxy that reads as a joint. A buyer who expected open crevices and receives black filler will reject the container.
Honey: oil, not stain
Honey is what most importers mean by “natural teak colour”. It is a penetrating oil — teak oil, or a linseed and tung blend with driers — worked into the grain and wiped back. Nothing sits on the surface like lacquer: the oil soaks into the fibre, darkens it, and leaves the grain readable under a warm amber-brown tone.
It is the default for export for three reasons. It is repairable: a scuff is sanded locally and re-oiled, and the patch blends within a week. It moves with the wood instead of cracking off it, which matters on a root that keeps adjusting to a new climate for a year. And it is the tone buyers recognise from showroom photography. The colour comes from the oil, not a dye, so two pieces from one batch will differ.
Honey oil also dries out. Indoors, expect to re-oil every six to twelve months; on a covered terrace in strong sun, every four to six months. The test is water: when a drop stops beading and starts to soak in, it is time. Selling honey as a permanent finish is how a good table gets a bad review in year two.

Black-wash: pigment in a binder
Black-wash is not paint and it is not burnt wood. It is pigment — black or a very dark brown — carried in a thin binder, worked into the sanded surface and wiped back so it stays in the pores and the softer grain. The result is a dark piece where the grain reads lighter than the field.
We sand to 180, raise the grain with water, sand again, then apply the wash in two passes, wiping each back before it sets, and seal on top. Done well, the piece looks like dark wood with a visible figure; done badly, it looks like black paint with sanding scratches under it.
Two failure points. Edge wear: pigment sits on the surface, so a corner that takes knocks goes pale within a season and cannot be touched up invisibly the way oil can. Sun: on an open terrace, ultraviolet light breaks the pigment down unevenly and grey shows first on upward faces. Black-wash belongs under a roof — hotel lobby, restaurant interior, covered veranda — not on a beach deck. A dark piece also hides grain defects, so a supplier can use a lower grade of root under black-wash than under natural.
The same table in three finishes: what it costs
These numbers are from our model list. Note the last column: the finish is nowhere in the freight arithmetic, because packed volume and FOB are set by the model, not the colour.
| Model | Size | CBM | FOB USD | Pcs / 20ft | FOB per CBM | Finish that suits it |
|---|---|---|---|---|---|---|
| Console Gold | 120 cm | 0.36 | 135 | 66 | USD 375 | Natural or honey |
| Live-edge coffee table | 120 × 80 cm | 0.38 | 145 | 62 | USD 382 | Natural, grain forward |
| Mawar coffee table | 120 cm | 0.65 | 135 | 36 | USD 208 | Black-wash |
| Teak Branch dining table | Ø 120 cm | 1.08 | 165 | 22 | USD 153 | Honey oil |
| Mawar dining table | Ø 150 cm | 1.69 | 340 | 14 | USD 201 | Honey or black-wash |
| Mawar dining table | Ø 200 cm | 2.43 | 650 | 9 | USD 267 | Honey, one-piece look |
The Teak Branch Ø 120 cm carries USD 153 of FOB value per cubic metre; the Mawar Ø 150 cm carries USD 201. A mixed load of eight Mawar Ø 150 (13.52 CBM) and nine Teak Branch Ø 120 (9.72 CBM) fills 23.24 CBM and leaves 0.56 for a Console Gold 120 cm at 0.36 — 18 pieces, 23.60 CBM, inside 23.8.
What the finish does change: weeks and rejects
Finish is free in freight and expensive in time. Natural is fastest through the workshop. Honey adds a day of oiling and two to three days of drying before packing, and the drying room is the bottleneck in the wet season. Black-wash adds two passes, a raise-and-sand cycle and a sealer, plus a longer cure; a black-wash piece packed soft will print the blanket into its surface. A buyer who switches finish after production starts loses one to two weeks.
Writing the finish on a purchase order
Five lines prevent most disputes. Name the finish and the product family: penetrating oil, pigment wash, or bare sanded. Give the sheen — matte, satin or gloss — because “natural” says nothing about sheen. State the sanding grit for visible faces. Say what happens to voids: open, clear-filled or black-filled. And name the maintenance product you will recommend, so nobody sells an incompatible wax on top of an oil. For a project order, add a sealed finished sample in the actual species and wash, plus photographs of the first three pieces off the line.
Which finish to choose
Natural for restaurants, beach clubs and any buyer who wants the root to look like a root and accepts grey. Honey for hotels, villas and retail programmes that need a warm tone and can carry a re-oiling interval. Black-wash for covered interiors where grain contrast is the design idea and edge wear will be light. None is better; each is a different promise, and the promise has to match the room the table will live in.
Request FOB prices and a load planBuild a container load →
Frequently asked questions
Is a honey finish a stain or an oil?
An oil. Honey is a penetrating oil worked into the grain and wiped back, so the colour sits in the fibre rather than on top of it. It darkens the wood and keeps the grain readable, and it can be repaired locally by sanding and re-oiling. A pigment stain sits in the pores and is harder to spot-repair.
Does the finish change the CBM or the FOB price?
No. Packed volume and FOB are set by the model and size. A Mawar Ø 150 cm is 1.69 CBM and USD 340 whether it ships natural, honey or black-wash, and a 20ft still loads 14 pieces.
Can black-wash teak root furniture go outdoors?
Under a roof, yes; on an open deck we advise against it. Pigment breaks down unevenly in ultraviolet light, grey shows first on upward faces, and worn edges cannot be touched up invisibly. For open terraces, natural or honey oil ages far better.
How often does honey-oiled teak root need re-oiling?
Indoors every six to twelve months; on a covered terrace in strong sun, every four to six months. The test is water: when a drop stops beading and soaks in, the oil has dried out. Apply a thin coat, wipe off the excess and cure for 24 hours.

Written by
Mr. August Praymunor — Overseas Marketing Director
CV. Nusantara Sourcing Agent · manufacturer and exporter of teak root furniture in Jepara, Central Java, Indonesia. We have shipped over 300 containers since 2016, loading 4×40’FCL per month for importers, hotel groups and interior contractors in Europe and North America. Every price and volume in this article comes from our own model list and shipping records.
export@teakrootfurniture.com · WhatsApp +62 852 0600 7878 · LinkedIn · Jl. RA Rukmini KM.02 Pekalongan RT.02/V, Tahunan, Jepara 59428, Central Java, Indonesia
Where to go next
FAQ: Sourcing Agent & Factory Visits
Do you provide sourcing-agent services or factory visits?
We manufacture and export our own furniture from Jepara, Indonesia. We do not run a sourcing-agency service (no daily fee, no commission, no multi-supplier tours). Buyers/importers are welcome to visit our workshop; for products outside our lines we can consolidate and cooperate with other suppliers.







0 comments: